Picture of B2.1-22-015:2002 STANDARD WELDING PROCEDURE SPECIFICATION (SWPS) FOR GAS TUNGSTEN ARC WELDING OF ALUMINUM, (M/P/S-22 TO M/P/S-22), 18 THROUGH 10 GAUGE, IN THE AS-WELDED CONDITION, WITH OR WITHOUT BACKING (HISTORICAL)

B2.1-22-015:2002 STANDARD WELDING PROCEDURE SPECIFICATION (SWPS) FOR GAS TUNGSTEN ARC WELDING OF ALUMINUM, (M/P/S-22 TO M/P/S-22), 18 THROUGH 10 GAUGE, IN THE AS-WELDED CONDITION, WITH OR WITHOUT BACKING (HISTORICAL)



Member Price: $264.00

Non-Member Price: $352.00

This standard contains the essential welding variables for aluminum in the thickness range of 10 through 18 gauge using manual gas tungsten arc welding. It cites the base metals and operating conditions necessary to make the weldment, the filler metal specifications, and the allowable joint designs for fillet welds and groove welds. ISBN 0-87171-687-9