Picture of B2.1-4-219:1999(R2009) STANDARD WELDING PROCEDURE SPECIFICATION (SWPS) FOR GAS TUNGSTEN ARC WELDING FOLLOWED BY SHIELDED METAL ARC WELDING OF CHROMIUM- MOLYBDENUM STEEL, (M-4/P-4, GROUP 1 OR 2), 1/8 THROUGH 1/2 INCH THICK

B2.1-4-219:1999(R2009) STANDARD WELDING PROCEDURE SPECIFICATION (SWPS) FOR GAS TUNGSTEN ARC WELDING FOLLOWED BY SHIELDED METAL ARC WELDING OF CHROMIUM- MOLYBDENUM STEEL, (M-4/P-4, GROUP 1 OR 2), 1/8 THROUGH 1/2 INCH THICK



Member Price: $264.00

Non-Member Price: $352.00

This standard contains the essential welding variables for chromium-molybdenum steel in the thickness range of 1/8 through 1/2 in. in the as-welded condition, or 1/8 in. through 1-1/2 in. in the postweld heat treated (PWHT) condition, using manual gas tungsten arc welding followed by manual shielded metal arc welding. It cites the base metals and operating conditions necessary to make the weldment, the filler metal specifications, and the allowable joint designs for groove welds. This welding procedure specification (WPS) was developed primarily for pipe applications.

Formats Member Price Non-Member Price Quantity
Printed Hard Copy
$264.00
$352.00
Download PDF
$264.00
$352.00