Picture of B2.1-1-233:2006 STANDARD WELDING PROCEDURE SPECIFICATION (SWPS) FOR ARGON PLUS 25% CARBON DIOXIDE SHIELDED GAS METAL ARC WELDING (SHORT CIRCUITING TRANSFER MODE) FOLLOWED BY ARGON PLUS  2% OXYGEN SHIELDED GAS METAL ARC WELDING (SPRAY TRANSFER MODE)

B2.1-1-233:2006 STANDARD WELDING PROCEDURE SPECIFICATION (SWPS) FOR ARGON PLUS 25% CARBON DIOXIDE SHIELDED GAS METAL ARC WELDING (SHORT CIRCUITING TRANSFER MODE) FOLLOWED BY ARGON PLUS 2% OXYGEN SHIELDED GAS METAL ARC WELDING (SPRAY TRANSFER MODE)



Member Price: $264.00

Non-Member Price: $352.00

This standard contains the essential welding variables for carbon steel in the thickness range of 1/8 through 1-1/2 inch, using Argon plus 25% Carbon Dioxide shielded gas metal arc welding (short circuiting transfer mode) for the root followed by Argon plus 2% Oxygen shielded gas metal arc welding (spray transfer mode) for the balance. It cites the basemetals and operating conditions necessary to make the weldment, the filler metal specifications, and the allowable joint designs for groove welds. This WPS was developed primarily for pipe applications. ISBN 0-87171-016-1

Formats Member Price Non-Member Price Quantity
Printed Hard Copy
$264.00
$352.00
Download PDF
$264.00
$352.00