Picture of B2.1-4-218:1999 STANDARD WELDING PROCEDURE SPECIFICATION FOR SMAW OF CHROMIUM - MOLYBDENUM STEEL, (M-4/P-4, GROUP 1 or 2), E8018-B2, 1/8 THROUGH 1/2 INCH THICK, AS-WELDED CONDITION, 1/8 THROUGH 1-1/2 INCH THICK, PWHT CONDITION (HISTORICAL)

B2.1-4-218:1999 STANDARD WELDING PROCEDURE SPECIFICATION FOR SMAW OF CHROMIUM - MOLYBDENUM STEEL, (M-4/P-4, GROUP 1 or 2), E8018-B2, 1/8 THROUGH 1/2 INCH THICK, AS-WELDED CONDITION, 1/8 THROUGH 1-1/2 INCH THICK, PWHT CONDITION (HISTORICAL)



Member Price: $264.00

Non-Member Price: $352.00

This standard contains the essential welding variables for chromium-molybdenum steel in the thickness range of 1/8 through 1/2 in. in the as-welded condition, or 1/8 in. through 1-1/2 in. in the postweld heat treated (PWHT) condition, using manual shielded metal arc welding. It cites the base metals and operating conditions necessary to make the weldment, the filler metal specifications, and the allowable joint designs for groove welds. This welding procedure specification (WPS) was developed primarily for pipe applications. ISBN 0-87171-593-7

Formats Member Price Non-Member Price Quantity
Download PDF
$264.00
$352.00