B2.1-1/8-228:2023-STANDARD WELDING PROCEDURE SPECIFICATION (SWPS) FOR SMAW OF CARBON STEEL (M-1/P-1, GROUPS 1 OR 2) TO AUSTENITIC STAINLESS STEEL (M-8/P-8, GROUP 1), 1/8 IN [3 mm] THROUGH 1-1/2 IN [38 mm] THICK, E309(L)-15, -16, OR -17, IN THE AS-WELDED CONDITION, PRIMARILY PIPE APPS



Member Price: $264.00

Non-Member Price: $352.00

This standard contains the essential welding variables for welding carbon steel to austenitic stainless steel in the thickness range of 1/8 inch [3 mm] through 1-1/2 inch [38 mm], using manual shielded metal arc welding.

It cites the base metals and operating conditions necessary to make the weldment, the filler metal specifications, and the allowable joint designs for groove and fillet welds. This SWPS was developed primarily for pipe applications.


Formats Member Price Non-Member Price Quantity
Printed Hard Copy
$264.00
$352.00
Download PDF
$264.00
$352.00