Picture of B2.1-8-024:2023 STANDARD WELDING PROCEDURE SPECIFICATION (SWPS) FOR GAS TUNGSTEN ARC WELDING OF AUSTENITIC STAINLESS STEEL (M-8/P-8, GROUP 1), 1/16 IN THROUGH 1-1/2 IN THICK, ER3XX, AS-WELDED CONDITION PRIMARILY PLATE AND STRUCTURAL APPLICATIONS

B2.1-8-024:2023 STANDARD WELDING PROCEDURE SPECIFICATION (SWPS) FOR GAS TUNGSTEN ARC WELDING OF AUSTENITIC STAINLESS STEEL (M-8/P-8, GROUP 1), 1/16 IN THROUGH 1-1/2 IN THICK, ER3XX, AS-WELDED CONDITION PRIMARILY PLATE AND STRUCTURAL APPLICATIONS



Member Price: $264.00

Non-Member Price: $352.00

This standard contains the essential welding variables for austenitic stainless steel in the thickness range of 1/16 in [1.5 mm] through 1-1/2 in [38 mm], using manual gas tungsten arc welding.

It cites the base metals and operating conditions necessary to make the weldment, the filler metal specifications, and the allowable joint designs for fillet and groove welds.

This SWPS was developed primarily for plate and structural applications.

Formats Member Price Non-Member Price Quantity
Printed Hard Copy
$264.00
$352.00
Download PDF
$264.00
$352.00