Picture of B2.1-8-009:2002 (S2022) - STANDARD WELDING PROCEDURE SPECIFICATION (SWPS) FOR GAS TUNGSTEN ARC WELDING OF AUSTENITIC STAINLESS STEEL (M-8, P-8, OR S-8), 18 THROUGH 10 GAUGE, IN THE AS-WELDED CONDITION, WITH OR WITHOUT BACKING

B2.1-8-009:2002 (S2022) - STANDARD WELDING PROCEDURE SPECIFICATION (SWPS) FOR GAS TUNGSTEN ARC WELDING OF AUSTENITIC STAINLESS STEEL (M-8, P-8, OR S-8), 18 THROUGH 10 GAUGE, IN THE AS-WELDED CONDITION, WITH OR WITHOUT BACKING



Member Price: $264.00

Non-Member Price: $352.00

This standard contains the essential welding variables for welding austenitic stainless steel in the thickness range of 18
through 10 gauge using manual gas tungsten arc welding. It cites the base metals and operating conditions necessary to
make the weldment, the filler metal specifications, and the allowable joint designs for fillet welds and groove welds.