Picture of B2.1-5A-222:2022 STANDARD WELDING PROCEDURE SPECIFICATION (SWPS) FOR GAS TUNGSTEN ARC WELDING OF CHROMIUM-MOLYBDENUM STEEL (M-5A/P-5A), ER90S-B3, 1/8 INCH [3 MM] THROUGH 1/2 INCH [13 MM] THICK, AS-WELDED CONDITION; 1/8 INCH THROUGH 3/4 INCH THICK,PRIMARILY PIPE APPLICATIONS

B2.1-5A-222:2022 STANDARD WELDING PROCEDURE SPECIFICATION (SWPS) FOR GAS TUNGSTEN ARC WELDING OF CHROMIUM-MOLYBDENUM STEEL (M-5A/P-5A), ER90S-B3, 1/8 INCH [3 MM] THROUGH 1/2 INCH [13 MM] THICK, AS-WELDED CONDITION; 1/8 INCH THROUGH 3/4 INCH THICK,PRIMARILY PIPE APPLICATIONS



Member Price: $264.00

Non-Member Price: $352.00

This standard contains the essential welding variables for chromium-molybdenum steel in the thickness range of 1/8 inch [3 mm] through 1/2 inch [13 mm] in the as-welded condition; or 1/8 inch [3 mm] through 3/4 inch [19 mm] in the postweld
heat treated (PWHT) condition, using manual gas tungsten arc welding. It cites the base metals and operating conditions necessary to make the weldment, the filler metal specifications, and the allowable joint designs for groove welds.
This standard welding procedure specification (SWPS) was developed primarily for pipe applications.