B2.1-1-018:2021 Standard Welding Procedure Specification (SWPS) for Self-Shielded Flux Cored Arc Welding of Carbon Steel (M-1/P-1, Group 1 or 2) 1/8 inch [3 mm] through 1-1/2 inch [38 mm] Thick, E71T-8, in the As-Welded Condition, Primarily Plate and Structural Applications
Member Price: $264.00
Non-Member Price: $352.00
This standard contains the essential welding variables for carbon steel in the thickness range of 1/8 inch [3 mm] through
1-1/2 inch [38 mm], using semiautomatic self-shielded flux cored arc welding. It cites the base metals and operating conditions
necessary to make the weldment, the filler metal specifications, and the allowable joint designs for fillet and
groove welds. This SWPS was developed primarily for plate and structural applications.