Picture of B2.1-8-216:2001(R2012) STANDARD WELDING PROCEDURE SPECIFICATION FOR GTAW WITH CONSUMABLE INSERT ROOT FOLLOWED BY SHIELDED METAL ARC WELDING OF AUSTENITIC STAINLESS STEEL, (M-8/P-8/S-8, GROUP 1), 1/8 THROUGH 1-1/2 INCH THICK, IN3XX, ER3XX (HISTORICAL)

B2.1-8-216:2001(R2012) STANDARD WELDING PROCEDURE SPECIFICATION FOR GTAW WITH CONSUMABLE INSERT ROOT FOLLOWED BY SHIELDED METAL ARC WELDING OF AUSTENITIC STAINLESS STEEL, (M-8/P-8/S-8, GROUP 1), 1/8 THROUGH 1-1/2 INCH THICK, IN3XX, ER3XX (HISTORICAL)



Member Price: $264.00

Non-Member Price: $352.00

This standard contains the essential welding variables for austenitic stainless steel in the thickness range of 1/8 through 1-1/2 inch, using manual gas tungsten arc welding with consumable insert root followed by shielded metal arc welding. It cites the base metals and operating conditions necessary to make the weldment, the filler metal specifications, and the allowable joint designs for groove welds. This WPS was developed primarily for pipe applications.

Formats Member Price Non-Member Price Quantity
Printed Hard Copy
$264.00
$352.00
Download PDF
$264.00
$352.00